Ferrous Alloys

Type 348 Austenitic Stainless Steel

Application & Characteristics 
Preferred over Type 347 for nuclear components.
Chemical Composition (%)
Same as Type 347 except Ta 0.10 max.
Physical Properties
Melting Range (°F)2550 – 2600
Density (lbs/in³) 68F0.286
Thermal Expansion (in/in °Fx10 to the power of -6)9.4 (0 – 600F)
Electrical Resistivity (ohms/cir mil/ft.) 68F440
Mechanical Properties – Temper = A
Tensile Strength (psi x 10³)85
Yield Strength (psi x 10³)40
Elongation ( % )50
HardnessB85(Rockwell)
Mechanical Properties – Temper = H/2
Tensile Strength (psi x 10³)125
Yield Strength (psi x 10³)95
Elongation ( % )25
HardnessC20(Rockwell)
Mechanical Properties – Temper = H
Tensile Strength (psi x 10³)165
Yield Strength (psi x 10³)135
Elongation ( % )8
HardnessC30(Rockwell)

Request a quote from Asgard Engineering

You may like to contact Asgard Engineering with certain files and information such as Autocad files, images or word documents.

Contact us using the link below and you'll be able to e-mail and attach files and send relevant information  Thank you.

Request A Quote

Request a Quote

CLICK HERE FOR A QUOTE

You have Successfully Subscribed!