Ni-Span-C

Application & Characteristics 
Pressure-sensitive devices.
Chemical Composition (%)
Ni 42; Cr 5.4; Ti 2.4; Fe 48.5; Al 0.65 Allowable maximums; C 0.06; Mn 0.80; S 0.04; P 0.04; Si 1.00; Cu 0.20
Physical Properties
Melting Range (°F)2650 – 2700
Density (lbs/in³) 68F0.293
Thermal Expansion (in/in °Fx10 to the power of -6)4.5 (-50 – +150F)
Electrical Resistivity (ohms/cir mil/ft.) 68F611
Mechanical Properties – Temper = A
Tensile Strength (psi x 10³)90
Yield Strength (psi x 10³)40
Elongation ( % )40
HardnessB75(Rockwell)
Mechanical Properties – Temper = H/2
Tensile Strength (psi x 10³)120
Yield Strength (psi x 10³)115
Elongation ( % )20
HardnessB95(Rockwell)
Mechanical Properties – Temper = H
Tensile Strength (psi x 10³)130
Yield Strength (psi x 10³)125
Elongation ( % )6
HardnessC25(Rockwell)

Request a quote from Asgard Engineering

You may like to contact Asgard Engineering with certain files and information such as Autocad files, images or word documents.

Contact us using the link below and you'll be able to e-mail and attach files and send relevant information  Thank you.

Request A Quote