Copper Alloys

Deoxidised Copper Low Phospherous

Application & Characteristics 
Tubing exposed to refrigerants or hydrocarbons when high thermal conductivity is desirable.
Chemical Composition (%)
Cu 99.90 Min; P 0.012 Max.
Physical Properties
Melting Range (°F)1981
Density (lbs/in³) 68F0.323
Thermal Expansion (in/in °Fx10 to the power of -6)9.8 (68-572F)
Electrical Resistivity (ohms/cir mil/ft.) 68F10.7
Mechanical Properties – Temper = A
Tensile Strength (psi x 10³)32
Yield Strength (psi x 10³)10
Elongation ( % )45
HardnessF40(Rockwell)
Mechanical Properties – Temper = H/2
Tensile Strength (psi x 10³)45
Yield Strength (psi x 10³)35
Elongation ( % )20
HardnessF80(Rockwell)
Mechanical Properties – Temper = H
Tensile Strength (psi x 10³)50
Yield Strength (psi x 10³)45
Elongation ( % )10
HardnessB50(Rockwell)

Request a quote from Asgard Engineering

You may like to contact Asgard Engineering with certain files and information such as Autocad files, images or word documents.

Contact us using the link below and you'll be able to e-mail and attach files and send relevant information  Thank you.

Request A Quote