Metal Properties

Type 348 Austenitic Stainless Steel

 
Application & Characteristics
Preferred over Type 347 for nuclear components.
 
Chemical Composition (%)
Same as Type 347 except Ta 0.10 max.
 
Physical Properties
Melting Range (°F) 2550 – 2600
Density (lbs/in³) 68F 0.286
Thermal Expansion (in/in °Fx10 to the power of -6) 9.4 (0 – 600F)
Electrical Resistivity (ohms/cir mil/ft.) 68F 440
 
Mechanical Properties – Temper = A
Tensile Strength (psi x 10³) 85
Yield Strength (psi x 10³) 40
Elongation ( % ) 50
Hardness B85(Rockwell)
 
Mechanical Properties – Temper = H/2
Tensile Strength (psi x 10³) 125
Yield Strength (psi x 10³) 95
Elongation ( % ) 25
Hardness C20(Rockwell)
 
Mechanical Properties – Temper = H
Tensile Strength (psi x 10³) 165
Yield Strength (psi x 10³) 135
Elongation ( % ) 8
Hardness C30(Rockwell)